Skim Coat & Wall Putty Additives: Smooth Finish Without Powdering or Cracking

Grades and starting dosages for cement-based, gypsum-based and exterior wall putty.

Improve water retention, smooth application and open time for better finishing performance.

Enhance adhesion, flexibility and crack resistance in cement-based wall formulations.

Improve anti-sagging performance and application consistency for smoother construction.

LANDU: Your Skim Coat & Wall Putty Additives Manufacturer

Wall putty is applied in layers of 1–3 mm, so it dries faster and is judged more harshly than any other mortar: powdering, hairline cracks and trowel drag are visible the next morning. The fix is almost never more cement — it is the right cellulose ether grade for the layer thickness, enough polymer to bind the surface, and a starch ether to make the putty move under the blade. This page gives the grades and starting dosages for cement-based, gypsum-based and exterior putties.

Three putty systems, three different additive briefs

SystemBinderWhere it is usedWhat the additive package must doReference standard
Cement-based skim coat / exterior puttyWhite or grey cement + limestone fillerExterior façades, wet rooms, concrete leveling before paintWater retention on absorbent substrates, adhesion to concrete and AAC, water resistance, crack controlEN 998-1 (OC/GP render types)
Gypsum-based finishing puttyGypsum hemihydrate (± lime)Interior walls and ceilings, plasterboard joints and skimOpen time control, sandability, no shrinkage cracking, smooth white surfaceEN 13279-1 (C6 thin-coat, C7 finishing plaster)
Polymer-modified interior puttyCement or gypsum with 3–8 % RDPHigh-end interior finishing, machine-applied skimZero powdering, flexibility over joints, fine textureEN 998-1 / EN 13279-1 as applicable

Grade selection

Landercoll® cellulose ether. The technical data sheets list “skim coat / wall putty (powder form)” for K75, K100, EM60, EM80 and EM100, “skim coat / wall putty” for K150, K200, K200H and EM200, and “wall putty / skim coat” for EM100H. For ready-mixed paste putty the TDS recommends the surface-treated, delayed-solubility grades K40HS and K75HS (“latex-based and paste application, wall putties, joint fillers”). For gypsum putty the dedicated HEMC grades are ME3570-G and ME4080-G (“gypsum-based wall putty / skim coat”). Viscosities are Brookfield RV, 2 % solution, 20 °C.

Putty typeCellulose ether (viscosity)Starting dosageNotes
Interior cement putty, hand-applied, 1–2 mmK75 (35,000–40,000) · K100 (45,000–60,000) / EM80 (35,000–45,000) · EM100 (45,000–60,000)0.25–0.35 %Standard putty grades on the TDS; K200 (65,000–80,000) for very absorbent blockwork
Exterior cement putty, 2–3 mmK150 (55,000–65,000) · K200H / EM100H (45,000–60,000)0.30–0.40 %K150: water retention “very high”; EM100H: sag resistance “excellent”, heat resistance “excellent”
Machine-sprayed skim coatEM60 (30,000–40,000) · EM80 / K750.25–0.35 %Medium viscosity for pumpability; combine with ST2109 or ST3152 starch ether for anti-sag
Gypsum finishing puttyME3570-G (35,000–45,000) · ME4080-G (30,000–40,000)0.15–0.30 %HEMC modified for gypsum: water retention “excellent”, final consistency “superior”; K100 / EM100 also list gypsum plasters
Ready-mixed (paste) puttyK40HS (20,000–24,000) · K75HS (35,000–40,000)0.3–0.5 %Surface-treated for delayed dissolution and lump-free mixing in water; combine with Landercoll® HEC for storage stability

Accurate® redispersible polymer powder

Grade familyGrades (TDS Tg / MFFT)Typical dosageUse
Rigid VAE5011N, 4012N (Tg 10 ± 5 °C / MFFT 4 °C)1–2 %Interior putty: hardness, no powdering, good sandability — both TDS list wall putty
Semi-flexible VAE4025N (Tg 0 °C / MFFT 1 °C)2–3 %Exterior putty on render, cement board, AAC
Flexible5045N (Tg −10 ± 5 °C / MFFT 0 °C), 9055E acrylic–silane (Tg −15 °C)3–5 %Putty over ETICS base coats and substrates with movement; 5045N TDS lists wall putty / skim coat, 9028E/9055E list thermal-insulation putty systems
Hydrophobic8032H (medium hydrophobic), 8035H (strong hydrophobic), 8048H (very strong, instant-dissolving)2–4 %Wet rooms and façades exposed to driving rain; 8032H and 8035H TDS list skim coat, 8048H lists waterproof putty

NOVASTAR® specialty additives

  • Starch ether (HPS), 0.03–0.08 %: ST1506-A (5 % viscosity 500–3,500 mPa·s), ST1506-B (100–800 mPa·s) and ST1403B (300–1,000 mPa·s) are the putty and hand-plaster grades; ST3547 (200–1,500 mPa·s, low ash) and ST3206 (500–2,000 mPa·s) are universal grades for putty, plaster and adhesive mortars. Instant thickening, creamy consistency, less trowel drag, better anti-sag.
  • SHP75 / SHP80 silicone hydrophobic powder, 0.2–0.5 % (TDS range 0.1–0.5 %): water-repellent exterior putty, reduced capillary absorption and efflorescence, limited impact on mechanical properties, UV-stable silane/resin active.
  • Powder defoamer P805 (standard), P806 (alkali-resistant) or P807 (low-temperature), 0.1–0.2 %: removes pinholes in machine-mixed and sprayed putty.
  • Gypsum retarder NOVASTAR® P300 (amino-acid type, TDS dosage 0.05–0.3 % of binder) or P400 / AR-P (modified amino-acid type, TDS dosage 0.001–0.3 %; AR-P alkali-resistant for lime-containing systems): working-time control in gypsum putty; most putties settle between 0.02 and 0.1 %.

Dosages are percentages of the total dry mix for laboratory starting points; the technical data sheets do not prescribe dosages. Confirm with your binder and filler.

Troubleshooting on site

DefectWhat is happeningFormulation fix
Powdering / chalking after dryingWater left the layer before the binder hydrated; too little polymer at the surfaceRaise cellulose ether by 0.05 % or move to K150 / EM100H; add 1–2 % rigid RDP (5011N); check filler/binder ratio
Hairline map crackingThick single coat, fast drying, high filler contentLimit coat to ≤ 2 mm per pass; K150 or EM100H for water retention; 2–3 % 4025N; add 0.1 % PP fibre 3 mm for exterior
Sagging on walls, slumping in the bucketViscosity too low for layer thickness; excess waterEM100H or K200 (sag resistance “excellent”); 0.05 % ST1506-A; reduce water
Putty “rolls” or drags under the trowelCellulose ether viscosity too high; no starch etherStep down one viscosity (K200 → K100 → K75); add ST1506-B or ST3547
Hard to sandToo much RDP or flexible RDP in an interior puttyReduce to 1–2 % rigid RDP (5011N / 4012N)
Pinholes, bubblesAir entrained during high-speed mixing or spraying0.1–0.2 % P805 (P806 in high-alkali cement putty); slower mixer
Lumps when mixing paste puttyStandard cellulose ether dissolves on contact and agglomeratesSurface-treated K40HS / K75HS (delayed solubility: “yes” on the TDS)
Yellow or dark spots in white puttyCement or filler impurities, not the additiveChange to white cement / low-iron limestone; cellulose ether and RDP are white to off-white powders
Blistering or peeling on exterior puttyWater uptake and freeze; weak bond to renderSHP 0.3 %; hydrophobic RDP 8035H or 8048H; prime absorbent substrate
Short working time of gypsum puttySet not controlledGypsum retarder P300 at 0.05 % or P400 at 0.03 %; ME3570-G cellulose ether

Our field guide Why wall putty fails on site and the test-based article Wall putty powdering after drying go deeper into each case.

HPMC or RDP — which one is missing?

Formulators often ask whether a powdering putty needs more cellulose ether or more polymer. The quick test: wet the powdered surface. If it re-hardens, the cement never hydrated — add water retention. If it stays soft, the binder is fine but the surface is unbound — add RDP. The full comparison is in HPMC vs RDP in wall putty.

Starting formulations (laboratory basis, dry mix)

ComponentInterior cement puttyExterior cement puttyGypsum finishing putty
White cement 42.525–30 %30–35 %—
Gypsum hemihydrate——60–70 %
Limestone / heavy calcium carbonate60–70 %55–60 %25–35 %
Light calcium carbonate / talc3–5 %3–5 %3–5 %
Landercoll® cellulose etherK100 0.30 %EM100H 0.35 %ME3570-G 0.20 %
Accurate® RDP5011N 1.5 %4025N 2.5 %5011N 0.5–1 %
NOVASTAR® starch etherST1506-B 0.05 %ST3547 0.05 %ST1506-A 0.03 %
NOVASTAR® SHP75 / SHP80—0.3 %—
NOVASTAR® gypsum retarder P400——0.02–0.05 %

These are starting points used in our application laboratory, not finished recipes; raw-material sources and local standards require adjustment and testing.

Products referenced on this page

Working with LANDU

LANDU has produced cellulose ethers since 2011 and today runs three production bases in Shandong with 75,000 t annual capacity across Landercoll® cellulose ethers, Accurate® RDP and NOVASTAR® additives. The portfolio is REACH-compliant and manufactured under ISO 9001. Putty manufacturers in more than 60 countries use our grades; in Europe we deliver from stock through partners in several countries, including Greece, Spain and Italy. Cellulose ether ships in 25 kg bags on 500 or 600 kg pallets, RDP in 25 kg bags on 600–1,300 kg pallets (neutral or OEM bags available), with a lead time of 7–15 working days for factory shipments.

Skim Coat & Wall Putty Additives: Frequently Asked Questions

Answers on additive selection, testing, samples and supplier qualification.

What cellulose ether viscosity is right for wall putty?

For hand-applied interior putty, 45,000–60,000 mPa·s Brookfield (Landercoll® K100 / EM100; 85,000–110,000 mPa·s on the NDJ-1 scale) at 0.25–0.35 % is the usual starting point. Machine-sprayed skim coats work better with 30,000–45,000 mPa·s grades (EM60, EM80, K75); very absorbent blockwork may need K200.

How much RDP does a wall putty need?

Interior putty: 1–2 % of a rigid grade (5011N or 4012N) to stop powdering while keeping sandability. Exterior putty: 2–3 % semi-flexible 4025N, rising to 3–5 % flexible 5045N or 9055E over insulation systems. Above 5 % the putty becomes difficult to sand and the cost rises quickly.

Can the same additive package be used for cement and gypsum putty?

No. Gypsum sets by crystallisation and is sensitive to cellulose ether type and dosage; use the gypsum HEMC grades ME3570-G or ME4080-G at 0.15–0.30 % plus a retarder. Cement putty tolerates higher cellulose ether dosages and benefits more from RDP.

Why does my exterior putty crack while the same recipe works indoors?

Sun, wind and absorbent render remove water three to five times faster outdoors. Move from K100 to K150 or EM100H, add 0.05 % starch ether to allow a thinner coat, and raise RDP to 2.5–3 % to carry shrinkage stress.

Is starch ether necessary if I already use HPMC?

Not necessary, but 0.03–0.08 % of a putty grade such as ST1506-B or ST3547 changes the trowel feel noticeably: less drag, better anti-sag, and usually 1–2 % less water, which in turn reduces shrinkage.

Do you supply white, low-ash grades for white putty?

Yes. Landercoll® grades are white to off-white powders with residue on ignition ≤ 5 % (EM100H ≤ 3 %); Accurate® RDP is white to light beige. Colour problems in finished putty almost always come from grey cement or iron-bearing filler.

What does HPMC do in skim coat and wall putty?

Three jobs. It holds the mixing water in a 1–3 mm layer on an absorbent wall long enough for the cement to hydrate, which is what stops powdering. It sets the consistency so the putty moves under the blade without dragging. And it gives the yield stress that keeps a 2–3 mm coat on a vertical surface. Starting dosage 0.25–0.35 % of the dry mix; the grades whose TDS list putty are Landercoll® K75, K100, K150 and K200 and the HEMC grades EM60, EM80, EM100, EM100H and EM200.

HPMC or HEMC (MHEC) for wall putty: which is better?

At room temperature they retain water and thicken in the same way. HEMC (MHEC) has a higher thermal gel point, so it keeps its viscosity and open time in hot workshops and on sun-warmed walls above about 30 ℃, and at equal viscosity it usually gives a slightly smoother trowel feel. HPMC is the lower-cost choice for interior putty applied in temperate conditions. Run K100 and EM100 in the same base mix and compare water retention, sag and sanding; the TDS pairs for putty are K75 / EM80 and K100 / EM100.

Why does wall putty powder after drying?

Powdering means the surface cement never hydrated: the wall pulled the water out before set, or there was too little binder to coat the filler. Check in this order: water retention (raise the cellulose ether to 0.30–0.35 %, or move from K75 to K100), binder-to-filler ratio, RDP (1–2 % rigid 5011N or 4012N binds the surface), then curing conditions (wind, direct sun, heated rooms). More cellulose ether does not rescue a mix that is short of binder. The full test sequence is in wall putty powdering after drying.

Request Samples and a Grade Recommendation

Tell us the putty type, layer thickness and the defect you are fighting.

We return a grade recommendation and starting dosage within two working days and ship 200–600 g samples free of charge.

LANDU-product-test-laboratories

Ask a Formulation Engineer

LANDU — Committed to Every Gram.